NO 등록일 제목 저자 저널
1 2024 Effect of ladle slag composition on evolution behavior of non-metallic inclusions in Si-killed 316L stainless steel S.C. Duan, T.S. Kim, J.H. Cho, and J.H. Park J. Alloys & Compd., (2024), to be published.
2 2024 Abatement of CO2 emissions by lowering hot metal ratio (HMR) in basic oxygen steelmaking (BOS) process K.H. Kim and J.H. Park Ironmaking & Steelmaking, vol. 51, (2024), to be published.
3 2024 Reoxidation Phenomena of Liquid Steel in Secondary Refining and Continuous Casting Processes – A Review (Invited review article, Prof. Piotr R. Scheller special issue) J.H. Park and Y.B. Kang Steel Res. Int., vol. 95, (2024), accepted, in press.
4 2024 Evolution Behavior of Non-metallic Inclusions in High-Al or Si Alloyed Steel reacting with CaO-Al2O3-FeO-SiO2-MgO Slag D.W. Kim, T.S. Kim, G.H. Park, and J.H. Park Metall. Mater. Trans. B, vol. 55B, (2024), accepted, in press.
5 2023 Characterization and formation mechanism of non-metallic inclusions in single bcc-phase high entropy alloy Y. Wang, S. Lin, Z. Dong, J.H. Park, Q. Wang, H. Ni, and W. Mu Mater. Charact., vol. 25, (2023), article no. 113299. (November)
6 2023 Casting microstructure and phase-specific deformation behavior of Ti-20Ni alloy containing Ti2Ni phase J.S. Kim, S.Y. Hong, K. Park, J.H. Park, and J.K. Kim Mater. Today Commun., vol. 36, (2023), article no. 106549, pp. 1-5. (August)
7 2023 Enhanced strength-ductility balance of the (CoCrFeNiMn)95.2Al3.2Ti1.6 high-entropy alloy by co-precipitation of the B2 and sigma phases G. Yang, J. Kang, J.K. Kim, and J.H. Park Mater. Sci. Eng. A, vol. 873, (2023), article no. 145039, pp. 1-8. (May)
8 2023 Effect of tundish flux on reoxidation behavior of Si-killed 316L stainless steel S.C. Duan, T.S. Kim, J.H. Cho, and J.H. Park J. Mater. Res. & Technol., vol. 24, (2023), pp. 5165-5176. (May)
9 2023 Effect of ferrochromium (FeCr) and ferroniobium (FeNb) alloys on inclusion and precipitate characteristics in austenitic stainless steels Y. Wang, C. Liu, H. Ni, A. Karasev, W. Mu, P.G. Jönsson, and J.H. Park J. Mater. Res. & Technol., vol. 25, (2023), pp. 4989-5002. (July)
10 2023 Novel applications of ferroalloys for manufacturing of ultra-clean CoCrFeMnNi high-entropy alloy by slagging method S.C. Duan, J.H. Cho, M.J. Lee, W. Mu, and J.H. Park J. Alloys & Compd., vol. 939, (2023), article no. 168692, pp. 1-12 (April)
11 2023 Effect of Manufacturing Conditions and Al Addition on Inclusion Characteristics in Co-based Dual-phase High Entropy Alloy Y. Wang, Y. Li, W. Wang, H. Kong, Q. Wang, J.H. Park, and W. Mu Metall. Mater. Trans. A, vol. 54A, (2023), no. 7, pp. 2715-2729
12 2023 Heterogeneous grain size and enhanced hardness by precipitation of the BCC particles in medium entropy Fe-Ni-Cr alloys G. Yang, J. Kang, A. Carsbring, W. Mu, P. Hedström, J.K. Kim, and J.H. Park J. Alloys & Compd., vol. 931, (2023), article no. 167580, pp. 1-11 (January)
13 2023 Effect of oxygen blowing on the competitive removal rate of silicon and iron from molten copper J. Park, S.K. Kwon, J.E. Lee, Y. Kang, and J.H. Park J. Mater. Res. & Technol., vol. 23, (2023), pp. 4634-4641. (March)
14 2022 Manufacturing an ultra-low-sulfur CoCrFeMnNi high-entropy alloy by slagging through induction melting with ferroalloys feedstock S.C. Duan, J. Kang, J.H. Cho, M.J. Lee, W. Mu, and J.H. Park J. Alloys & Compd., vol. 928, (2022), article no. 167080, pp. 1-9 (December)
15 2022 Desulfurization behavior of Si-killed 316L stainless steel melt by CaO-SiO2-CaF2-Al2O3-MgO slag T.S. Jeong, J.H. Cho, J.H. Heo and J.H. Park J. Mater. Res. & Technol., vol. 18, (2022), pp. 2250-2260. (May)
16 2022 Effect of slag composition on the distribution and separation behavior of arsenic between CaO-based slag and liquid copper J. Park, H.J. Kim and J.H. Park J. Hazard. Mater., vol. 436, (2022), article no. 129154, pp. 1-8. (August)
17 2022 Oxidation behavior of boron in 9CrMoCoB steel by CaF2-CaO-Al2O3-SiO2-B2O3 electroslag remelting (ESR) type slag S.C. Duan, M.J. Lee, D.S. Kim and J.H. Park J. Mater. Res. & Technol., vol. 17, (2022), pp. 574-585. (March)
18 2022 Influence of Al2O3 and SiO2 on the structure and viscosity of iron-compound bearing calcium-aluminosilicate slags T.S. Kim and J.H. Park J. Alloys & Compd., vol. 916, (2022), article no. 165328, pp. 1-9. (September)
19 2022 Effect of temperature on the slag/refractory interfacial reaction with directed reduced iron (DRI) addition in an electric arc furnace (EAF) process: Diffusional growth of magnesiowüstite layer by Boltzmann-Matano analysis J.H. Heo and J.H. Park Ceram. Int., vol. 48, (2022), no. 12, pp. 17217-17224. (June)
20 2022 Comparison of Oxidation Behavior of Various Reactive Elements in Alloys during Electroslag Remelting (ESR) Process: An Overview S.C. Duan and J.H. Park ISIJ Int., vol. 62, (2022), no. 8, pp. 1561-1572.
21 2022 Effect of Temperature on the Oxidation Behavior of Al and Ti in Inconel® 718 Alloy by ESR Slag with Different Amounts of CaO (DOI: 10.1007/s11837-021-05139-2) S.C. Duan, M.J. Lee, J.H. Park, and H.J. Guo JOM, vol. 74, (2022), no. 3, pp. 1228-1236.
22 2022 Effect of Physicochemical Properties of Slag on the Removal Rate of Alumina Inclusions in the Ruhrstahl-Heraeus (RH) Refining Conditions T.S. Kim, J. Yang and J.H. Park Metall. Mater. Trans. B, (2022), no. 4, pp. 2523-2533.
23 2022 Inclusion engineering in medium Mn steels: Effect of hot-rolling process on the deformation behaviors of oxide and sulfide inclusions Y. Wang, Y. Yang, Z. Dong, J.H. Park, Z. Mi, X. Mao and W. Mu Metall. Mater. Trans. B, (2022), no. 4, pp. 2182-2197.
24 2022 Effect of pyro-processing conditions on impurity removal and precious metal enrichment in waste printed circuit board (WPCB) recycling process J.H. Heo, J. Park and J.H. Park Resour. Conserv. Recycl., vol. 179, (2022), article no. 106068, pp. 1-12. (April)
25 2022 Interfacial reactions between magnesia refractory and electric arc furnace (EAF) slag with use of direct reduced iron (DRI) as raw material J.H. Heo and J.H. Park Ceram. Int., vol. 48, (2022), no. 4, pp. 4526-4538. (February)
26 2022 Oxidation behavior of boron in 9CrMoCoB steel by CaF2-CaO-Al2O3-SiO2-B2O3 slag during electroslag remelting (ESR) process S.C. Duan, M.J. Lee, D.S. Kim and J.H. Park J. Mater. Res. & Technol., vol. 17, (2022), pp. 574-585. (March)
27 2021 Effect of LCFeCr Alloy Addition on the Non-metallic Inclusions Characteristics in Ti-containing Ferritic Stainless Steel Y. Wang, M.K. Oh, T.S. Kim, A. Karasev, W. Mu, J.H. Park and P.G. Jönsson Metall. Mater. Trans. B, vol. 52B, (2021), no. 6, pp. 3815-3832.
28 2021 Desulfurization Behavior of Incoloy® 825 Superalloy by CaO-Al2O3-MgO-TiO2 Slag J.H. Cho, J. Martinsson, D. Sichen and J.H. Park Metall. Mater. Trans. B, vol. 52B, (2021), no. 6, pp. 3660-3670.
29 2021 Influence of slag composition and oxygen potential on thermodynamic behavior of vanadium in FeO-TiO2-MgO-SiO2-Al2O3 smelting slag and molten iron J.H. Heo, Y. Lee, H.S. Park, and J.H. Park J. Mater. Res. & Technol., vol. 15, (2021), pp. 5723-5732. (November)
30 2021 Inclusion engineering in Co-based duplex entropic alloys W. Wang, Y. Wang, W. Mu, J.H. Park, S. Sukenaga, H. Shibata, H. Larsson, H. Mao Mater. & Des., vol. 210, (2021), article number 110097, pp. 1-12. (November)
31 2021 Effect of fluorspar on the interfacial reaction between electric arc furnace slag and magnesia refractory: Competitive corrosion-protection mechanism of magnesiowüstite layer M.K. Oh and J.H. Park Ceram. Int., vol. 47, (2021), no. 14-15, pp. 20387-20398 (July)
32 2021 Evolution of the Non-Metallic Inclusions by Slag-Metal Reactions in Ti-containing Ferritic Stainless Steel Y. Wang, J.H. Cho, T.S. Jeong, A. Karasev, J.H. Park and P.G. Jönsson Metall. Mater. Trans. B, vol. 52B (2021), no. 6, pp. 3986-4001.
33 2021 Effect of Slag Composition on Dephosphorization and Foamability in the Electric Arc Furnace Steelmaking Process: Improvement of Plant Operation (MOLTEN2021 special issue) J.H. Heo and J.H. Park Metall. Mater. Trans. B, vol. 52B (2021), no. 6, pp. 3613-3623.
34 2021 Effect of White Mud Addition on Desulfurization Rate of Molten Steel (MOLTEN2021 special issue) T.S. Jeong, M.K. Oh, Y. Chung and J.H. Park Metall. Mater. Trans. B, vol. 52B (2021), no. 6, pp. 3596-3605.
35 2021 Non-metallic Inclusions in Different Ferroalloys and their Effect on the Steel Quality-A Review (MOLTEN2021 special issue) Y. Wang, A. Karasev, J.H. Park and P.G. Jönsson Metall. Mater. Trans. B, vol. 52B, (2021), no. 5, pp. 2892-2925
36 2021 Effect of Oxygen Blowing on Copper Droplet Formation and Emulsification Phenomena in Converting Process (MOLTEN2021 special issue) J.H. Park, J. Lee and J.H. Park J. Sustain. Metall., vol. 7, (2021), pp. 831-847. (September)
37 2021 Effect of Industrial Waste Fluxes (Red Mud and White Mud) on Dephosphorization and Refractory Corrosion: Applications to Electric Arc Furnace Steelmaking Process using Direct Reduced Iron (MOLTEN2021 special issue) M.K. Oh and J.H. Park Metall. Mater. Trans. B, vol. 52B (2021), no. 6, pp. 3583-3595.
38 2021 Viscosity-Structure Relationship of CaO-Al2O3-FetO-SiO2-MgO Ruhrstahl-Heraeus (RH) Refining Slag T.S. Kim and J.H. Park ISIJ Int., vol. 61, (2021), no. 3, pp. 724-733.
39 2021 Interfacial reactions and inclusion formations at an early stage of FeNb alloy additions to molten iron Y. Wang, A. Karasev, J.H. Park and P.G. Jönsson ISIJ Int., vol. 61, (2021), no. 1, pp. 209-218.
40 2021 Gold solubility in CaO-SiO2-Al2O3-Fe2O3 slags J.G. Yang, J.H. Park, J.Y. Kang, H.S. Park and J.H. Park JOM, vol. 73, (2021), no. 2, pp. 688-693.
41 2021 Design, synthesis, and characterization of a porous ceramic-supported CeO2 nanocatalyst for COx-free H2 evolution J. Lee, M. Lim, T.S. Kim, K.R. Park, J.S. Lee, H.B. Cho, J.H. Park and Y.H. Choa Appl. Surf. Sci., vol. 548, (2021), no. 149198, pp. 1-5. (May)
42 2021 Role of recrystallization and second phases on mechanical properties of a (CoCrFeMnNi)95.2Al3.2Ti1.6 high entropy alloy J. Kang, N. Park, J. Kim and J.H. Park Mater. Sci. Eng. A, vol. 814, (2021), article number 141249. (May)
43 2021 Influence of the Mg content on the austenite grain growth in offshore engineering steels considering TiN particle pinning and Mo solute drag effects X. Pan, J. Yang, Y. Zhang, J.H. Park and H. Ono Metall. Res. & Technol., (2021), no. 4, article number 409. (July/August)
44 2021 Effect of Tundish Flux on Compositional Changes in Non-metallic Inclusions in Stainless Steel Melts (invited to Development and Comprehension of Novel Experimental Technology for High Temperature Processing special issue) T.S. Kim, S.B. Lee and J.H. Park ISIJ Int., vol. 61 (2021), no. 12, pp. 2998-3007.
45 2021 Interfacial Phenomena and Inclusion Formation Behavior at Early Melting Stages of HCFeCr and LCFeCr Alloys in Liquid Iron Y. Wang, A. Karasev, J.H. Park, W. Mu, P.G. Jönsson Metall. Mater. Trans. B, vol. 52B (2021), no. 4, pp. 2459-73.
46 2020 Effect of CaF2 on phosphorus refining from molten steel by electric arc furnace slag using direct reduced iron (DRI) as a Raw Material M.K. Oh, T.S. Kim and J.H. Park Metall. Mater. Trans. B, vol. 51B, (2020), no. 6, pp. 3028-3038.
47 2020 Structural understanding of MnO-SiO2-Al2O3-Ce2O3 slag via Raman, 27Al NMR and X-ray photoelectron spectroscopies T.S. Kim, S.J. Jeong and J.H. Park Met. Mater. Int., vol. 26, (2020), no. 12, pp. 1872-1880.
48 2020 ‘Non-equilibrium state’ of grain boundaries in additively manufactured high-entropy CoCrFeMnNi alloy: a direct proof by tracer diffusion measurements N. Choi, V. Kulitckii, J. Kottke, B.T. Kavakbasi, J. Choe, J.H. Yu, S. Yang, J.H. Park, J.S. Lee, G. Wilde, S.V. Divinski J. Alloys & Compd., vol. 844, (2020), article number 155757, pp. 1-10. (December)
49 2020 Kinetic Modeling of Non-Metallic Inclusions Behavior in Molten Steel: A Review (selected as 2020 Editor’s Choice and invited paper for Metallurgical and Materials Transactions 50th anniversary collection) J.H. Park and L. Zhang Metall. Mater. Trans. B, vol. 51B, (2020), no. 6, pp. 2453-2482.
50 2020 Corrosion of stainless steel in a coal gasification plant S. Lee, S.Y. Hwang, S.W. Chung, S.J. Lee, Y. Yun, J.H. Park and M.J. Kim Mater. Perform., vol. 59, (2020), no. 9, pp. 44-49. (September)
51 2020 Effect of Fluorspar and Industrial Wastes (Red Mud and Ferromanganese Slag) on Desulfurization Efficiency of Molten Steel T.S. Jeong and J.H. Park Metall. Mater. Trans. B, vol. 51B, (2020), no. 5, pp. 2309-2320.
52 2020 Distribution characteristics of inclusions along with the surface sliver defect on the exposed panel of automobile: A quantitative electrolysis method X.Q. Pan, J. Yang, J.H. Park and H. Ono Int. J. Min. Metall. Mater., vol. 27, (2020), no. 11, pp. 1489-1498. (November)
53 2020 Formation behaviour of spinel-CaS multiphase inclusions in Ca-treated resulphurized steel during the ladle furnace process L. Krajnc, J. Burja, J. Medved, T.S. Kim and J.H. Park Mater. Technol., vol. 54, (2020), no. 4, pp. 559-565. (July)
54 2020 Thermodynamics of iron redox equilibria and viscosity-structure relationship of CaO-Al2O3-FetO melts T.S. Kim and J.H. Park J. Non-Cryst. Solids, vol. 542, (2020), article no. 120089, pp. 1-9. (August)
55 2020 Influence of manufacturing conditions on inclusion characteristics and mechanical properties of FeCrNiMnCo alloy N. Choi, N. Park, J. Kim, A.V. Karasev, P.G. Jonsson and J.H. Park Metals, vol. 10, (2020), article no. 1286, pp.1-16. (September)
56 2020 Prediction of Inclusion Evolution during Refining and Solidification of Steel: Computational Simulation and Experimental Confirmation J.H. Shin and J.H. Park Metall. Mater. Trans. B, vol. 51B, (2020), no. 3, pp. 1211-1224.
57 2020 Mechanical Performance Improvement by Nitrogen Addition in N-CoCrNi Compositionally Complex Alloys D.E. Jodi, N. Choi, J.H. Park and N. Park Metall. Mater. Trans. A, vol. 51A, (2020), no. 6, pp. 3228-3237.
58 2020 Improving the production efficiency of high-titania slag in Ti extraction process: fluxing effect on formation of pseudobrookite D.H. Kim, J.H. Heo, H.S. Park, J.K. Kim and J.H. Park Sci. Rep., vol. 10, (2020), article no. 6530, pp. 1-12. (April)
59 2020 Observations of FeO Reduction in Electric Arc Furnace Slag by Aluminum Black Dross: Effect of CaO Fluxing on Slag Morphology J.H. Heo, T.S. Kim, V. Sahajwalla and J.H. Park Metall. Mater. Trans. B, vol. 51B, (2020), no. 3, pp. 1201-1210
60 2020 Mechanism of Improving Heat-Affected Zone Toughness of Steel Plate with Mg Deoxidation after High-Heat-Input Welding L. Xu, J. Yang, J.H. Park and H. Ono Metals, vol. 10, (2020), article no. 162, pp.1-15. (January)
61 2020 Influence of calcium aluminate flux on reoxidation behaviour of molten steel during continuous casting process T.S. Kim, L. Holappa and J.H. Park Ironmaking & Steelmaking, vol. 47, (2020), no. 1, pp. 84-92.
62 2020 Strengthening of ultrafine-grained equiatomic CoCrFeMnNi high-entropy alloy by nitrogen addition D.E. Jodi, J.H. Park and N. Park : Mater. Lett., vol. 258, (2020), article no. 126772, pp. 1-4. (January)
63 2020 Investigation on the precipitate formation and behavior in nitrogen-containing equiatomic CoCrFeMnNi high-entropy alloy D.E. Jodi, J.H. Park, B. Straumal and N. Park Mater. Lett., vol. 258, (2020), article no. 126806, pp. 1-4. (January)
64 2019 Precipitate behavior in nitrogen-containing CoCrNi medium-entropy alloys D.E. Jodi, N. Park and J.H. Park Mater. Character., vol. 157, (2019), article no. 109888, pp. 1-9. (November)
65 2019 Mechanism of MgO dissolution in MgF2-CaF2-MF (M=Li or Na) melts: Kinetic analysis via in-situ high temperature confocal scanning laser microscopy (HT-CSLM) Y. Lee, J.G. Yang, D.J. Min and J.H. Park Ceram. Int., vol. 45, (2019), pp. 20251-20257. (November)
66 2019 Assessment of Physicochemical Properties of Electrical Arc Furnace Slag and their Effects on Foamability J.H. Heo and J.H. Park Metall. Mater. Trans. B, vol. 50B, (2019), no. 6, pp. 2959-2968.
67 2019 Influence of temperature on reaction mechanism of ilmenite ore smelting for titanium production D.H. Kim, T.S. Kim, J.H. Heo, H.S. Park and J.H. Park Metall. Mater. Trans. B, vol. 50B, (2019), no. 4, pp. 1830-1840.
68 2019 Massive recycling of waste mobile phones: Pyrolysis, physical treatment, and pyrometallurgical processing of insoluble residue H.S. Park, Y.S. Han and J.H. Park ACS Sustain. Chem. & Eng., vol. 7, (2019), no. 16, pp. 14119-14125. (August)
69 2019 Influence of exposure temperature on degradation of magnesia refractory by steel refining slags J.S. Han, Y. Chung and J.H. Park Met. Mater. Int., vol. 25, (2019), no. 5, pp. 1360-1365. (September)
70 2019 Crystallization and vitrification behavior of CaO-SiO2-FetO-Al2O3 slag: Fundamentals to use mineral wastes in production of glass ball J.H. Heo, J.W. Cho, H.S. Park and J.H. Park J. Clean. Prod., vol. 225, (2019), pp. 743-754. (July)
71 2019 Viscosity-structure relationship of alkaline earth silicate melts containing manganese oxide and calcium fluoride T.S. Kim and J.H. Park J. Am. Ceram. Soc., vol. 102, (2019), no. 8, pp. 4943-4955.
72 2019 Evolution of Oxide Inclusions in Si-Mn-Killed Steel during Protective Atmosphere Electroslag Remelting C. Shi and J.H. Park Metall. Mater. Trans. B, vol. 50B, (2019), no. 3, pp. 1139-1147.
73 2019 Corrosion behavior of a precipitation hardened Ni–Cr–Co–Mo alloy under partial slagging coal gasification conditions S. Lee, J.H. Park, S.Y. Hwang, S.W. Chung, S.J. Lee, Y. Yun and M.J. Kim Mater. Testing, vol. 61 (2019), no. 6, pp. 584-590.
74 2019 Effect of nitrogen on grain growth and formability of Ti-stabilized ferritic stainless steel M.H. Lee, R. Kim, and J.H. Park Sci. Rep., vol. 9, (2019), article no. 6369, pp. 1-11. (April)
75 2019 Interfacial reaction between magnesia refractory and “FeO”-rich slag: Formation of magnesiowüstitie protective layer J.S. Han, J.H. Heo, and J.H. Park Ceram. Int., vol. 45, (2019), no. 8, pp. 10481-10491. (June)
76 2019 Influence of Aluminum-Carbon Composite Pellet on FeO Reduction and Iron Recovery from Electric Arc Furnace Slag J.H. Heo, J.S. Yoo, Y. Chung and J.H. Park Metall. Mater. Trans. B, vol. 50B, (2019), no. 2, pp. 903-913.
77 2018 Effect of Direct Reduced Iron (DRI) on Dephosphorization of Molten Steel by Electric Arc Furnace Slag (selected as 2018 Metall. Mater. Trans. 2018 Editor’s Choice & TMS-EPD Science Awarded paper) J.H. Heo and J.H. Park Metall. Mater. Trans. B, vol. 49B, (2018), no. 6, pp. 3381-3389.
78 2018 Characterization of non-metallic inclusions and their influence on the mechanical properties of a FCC single-phase high-entropy alloy N. Choi, K.R. Lim, Y.S. Na, U. Glatzel and J.H. Park J. Alloys & Compd., vol. 763, (2018), pp. 546-557. (September)
79 2018 Thermodynamics of Fluoride-based Molten Fluxes for Extraction of Magnesium through Low Temperature Solid Oxide Membrane (LT-SOM) Process Y. Lee, J.G. Yang, and J.H. Park Calphad, vol. 62, (2018), pp. 232-237. (September)
80 2018 Synergistic effect of nitrogen and refractory material on TiN formation and equiaxed grain structure of ferritic stainless steel (IMPROWYS2017 special issue) M.H. Lee and J.H. Park Metall. Mater. Trans. B, vol. 49B, (2018), no. 3, pp. 877-893.
81 2018 Use of Industrial Waste (Al-Dross, Red mud, Mill scale) as Fluxing Agents in the Sulfurization of Fe-Ni-Cu-Co Alloy by Carbothermic Reduction of Calcium Sulfate J.H. Heo, E.H. Jeong, C.W. Nam, K.H. Park and J.H. Park Metall. Mater. Trans. B, vol. 49B, (2018), no. 3, pp. 939-943.
82 2018 Influence of CaF2 in calcium aluminate based slag on degradation of magnesia refractory J.S. Han, J.G. Kang, J.H. Shin, Y. Chung and J.H. Park Ceram. Int., vol. 44, (2018), no. 11, pp. 13197-13204. (August)
83 2018 Corrosion behavior of Hastelloy® C–4® Ni–Cr–Mo–Fe alloys for coal gasification syngas plants S. Lee, M.J. Kim, J.H. Park, S.H. Hwang, S.W. Chung, S.J. Lee and Y. Yun Mater. Testing, vol. 60 (2018), no. 2, pp. 156-162.
84 2018 Effect of CaF2 content in refining slag on formation behavior of spinel inclusion in Ni-Cr-V alloyed special steel (invited paper, selected as Hot article) J.H. Shin and J.H. Park J. Iron Steel Res. Int., vol. 25, (2018), no. 2, pp. 157-163.
85 2018 Manganese Recovery by Silicothermic Reduction of MnO in BaO-MnO-MgO-CaF2 (-SiO2) Slag J.H. Heo and J.H. Park Metall. Mater. Trans. B, vol. 49B, (2018), no. 2, pp. 514-518.
86 2018 Effect of CaO/Al2O3 ratio of ladle slag on formation behavior of inclusions in Mn and V alloyed steel J.H. Shin and J.H. Park ISIJ Int., vol. 58, (2018), no. 1, pp. 88-97.
87 2018 Formation mechanism of oxide-sulfide complex inclusions in high-sulfur containing steel melts J.H. Shin and J.H. Park Metall. Mater. Trans. B, vol. 49B, (2018), no. 1, pp. 311-324.
88 2017 Inclusions in stainless steels – a review (invited review paper) J.H. Park and Y. Kang Steel Res. Int., vol. 88, (2017), pp. 1700130 (1-26).
89 2017 Method of recycling titanium scrap via the electromagnetic cold crucible technique coupled with calcium treatment B.M. Moon, J.H. Seo, H.J. Lee, K.H. Jung, J.H. Park, and H.D. Jung J. Alloys & Compd., vol. 727, (2017), pp. 931-939. (December)
90 2017 Modification of Inclusions in Molten Steel by Mg-Ca Transfer from Top Slag: Experimental Confirmation of the 'Refractory-Slag-Metal-Inclusion (ReSMI)' Multiphase Reaction Model J.H. Shin and J.H. Park Metall. Mater. Trans. B, vol. 48B, (2017), no. 6, pp. 2820-2825.
91 2017 Corrosion-Erosion Behavior of MgAl2O4 Spinel Refractory in Contact with High MnO Slag avior of MgAl2O4 Spinel Refractory in Contact with High MnO Slag J. Jeon, Y. Kang, J.H. Park, and Y. Chung Ceram. Int., vol. 43 (2017), no. 17, pp. 15074-15079. (December)
92 2017 Thermochemical analysis for the reduction behavior of FeO in EAF slag via aluminothermic smelting reduction (ASR) process: Part I. Effect of aluminum on Fe & Mn recovery J.H. Heo and J.H. Park Calphad, vol. 58, (2017), pp. 219-228. (September)
93 2017 Thermochemical analysis for the reduction behavior of FeO in EAF slag via aluminothermic smelting reduction (ASR) process: Part II. Effect of aluminum dross and lime fluxing on Fe and; Mn recovery J.H. Heo and J.H. Park Calphad, vol. 58, (2017), pp. 229-238. (September)
94 2017 Vitrification of red mud with mine wastes through the melting and granulation process – application to ceramic ball H.S. Park and J.H. Park J. Non-Cryst. Solids, vol. 475 (2017), pp. 129-135. (November)
95 2017 Distribution Behavior of Aluminum and Titanium between Nickel-based Alloys and Molten Slags in Electro Slag Remelting (ESR) Process J.G. Yang and J.H. Park Metall. Mater. Trans. B, vol. 48B, (2017), no. 4, pp. 2147-2156.
96 2017 Effect of Rice Husk Insulation Powder on the Reoxidation Behavior of Molten Steel in Continuous Casting Tundish T.S. Kim, Y. Chung, L. Holappa and J.H. Park Metall. Mater. Trans. B, vol. 48B, (2017), no. 3, pp. 1736-1747.
97 2017 Effect of slag chemistry on desulfurization kinetics in secondary refining process J.G. Kang, J.H. Shin, Y. Chung, and J.H. Park Metall. Mater. Trans. B, vol. 48B, (2017), no. 4, pp. 2123-2135.
98 2017 Relationship between sulfide capacity and structure of MnO-SiO2-Al2O3-Ce2O3 system S.J. Jeong, T.S. Kim and J.H. Park Metall. Mater. Trans. B, vol. 48B, (2017), no. 1, pp. 545-553.
99 2017 Novel Design of Ferronickel Smelting Slag by Utilizing Red Mud as a Fluxing Agent: Thermochemical Computations and Experimental Confirmation H.S. Park, M.C. Ha, M.S. Kim, J.H. Heo, and J.H. Park Calphad, vol. 56, (2017), pp. 185-195. (March)
100 2017 Effect of initial iron content in a zinc bath on the dissolution rate of solid iron during hot dip galvanizing process S.M. Lee, S.K. Lee, D.J. Paik and J.H. Park Metall. Mater. Trans. A, vol. 48A, (2017), no. 4, pp. 1788-1796.
101 2017 Corrosion behavior of welded Ni-Co-Cr-Si alloys during exposure in integrated coal gasification combined cycle syngas plants S. Lee, M.J. Kim, J. Lee, J.H. Park, S.H. Kang, S.J. Lee and Y. Yun Mater. Testing, vol. 59 (2017), no. 1, pp. 16-21.
102 2017 TEM characterization of a TiN-MgAl2O4 epitaxial interface J.S. Park, D.H. Kim and J.H. Park J. Alloys & Compd., vol. 695, (2017), pp. 476-481. (February)
103 2017 Refractory-Slag-Metal-Inclusion Multiphase Reactions Modeling using Computational Thermodynamics: Kinetic Model for Prediction of Inclusion Evolution in Molten Steel (Christopher W. Bale Symposium special issue) J.H. Shin, Y. Chung and J.H. Park Metall. Mater. Trans. B, vol. 48B, (2017), no. 1, pp. 46-59.
104 2016 Effect of halide flux on physicochemical properties of MgCl2–based molten salts for accelerating zirconium production: Thermodynamic assessment J.H. Shin and J.H. Park Metall. Mater. Trans. E, vol. 3E, (2016), no. 3, pp. 218-226.
105 2016 Recovery of iron and removal of heavy metals from waste copper slag via novel aluminothermic smelting reduction (ASR) process J.H. Heo, Y. Chung, and J.H. Park J. Clean. Prod., (2016), vol. 137, pp. 777-787. (November)
106 2016 Effect of physicochemical properties of slag and flux on the removal rate of oxide inclusions from molten steel J.S. Park and J.H. Park Metall. Mater. Trans. B, vol. 47B, (2016), no. 6, pp. 3225-3230.
107 2016 Sulfurization of Fe-Ni-Cu-Co Alloy to Matte Phase by Carbothermic Reduction of Calcium Sulfate E.H. Jeong, C.W. Nam, K.H. Park and J.H. Park Metall. Mater. Trans. B, vol. 47B, (2016), no. 2, pp. 1103-1112.
108 2016 Effect of energy input on the characteristics of AISI H13 and D2 tool steels deposited by a directed energy deposition process J.S. Park, J.H. Park, M.G. Lee, J.H. Sung, K.J. Cha and D.H. Kim Metall. Mater. Trans. A, vol. 47A, (2016), no. 5, pp. 2529-2535.
109 2016 Initial wetting and spreading rate between SiC and CaO-SiO2-MnO slag J. Park, J.M. Jeon, K. Lee, J.H. Park and Y. Chung Metall. Mater. Trans. B, vol. 47B, (2016), no. 3, pp. 1832-1838.
110 2016 Thermodynamic behavior of manganese oxide in lime-based manganese smelting slags C.H. Eom, S.H. Lee, J.G. Park, J.H. Park and D.J. Min ISIJ Int., vol. 56, (2016), no. 1, pp. 37-43.
111 2015 Influence of Refractory-Steel Interfacial Reaction on the Formation Behavior of Inclusion in Ce-containing Stainless Steel Melt (Sawamura Awarded paper) S.K. Kwon, J.S. Park, and J.H. Park ISIJ Int., vol. 55, (2015), no. 12, pp. 2589-2596.
112 2015 Influence of the oxygen partial pressure and the boron content on the behavior of boron in calcium silicate melts S. Lee, E.J. Jung, J.H. Park and D.J. Min J. Non-Cryst. Solids, vol. 429, (2015), pp. 54-60. (December)
113 2015 Thermodynamics of gold dissolution behavior in CaO-SiO2-Al2O3-MgOsat Slag System Y.S. Han, D.R. Swinbourne, and J.H. Park Metall. Mater. Trans. B, vol. 46B, (2015), no. 6, pp, 2449-2557.
114 2015 Thermodynamic stability of spinel phase at the interface between alumina refractory and CaO-SiO2-CaF2-MgO-Al2O3-MnO slags J.S. Park, D.H. Kim and J.H. Park J. Am. Ceram. Soc., vol. 98, (2015), no. 6, pp. 1974-1981
115 2015 Variation in the chemical driving force for intragranular nucleation in the weld metal during multi-pass welding Y. Kang, K. Han, J.H. Park and C. Lee Metall. Mater. Trans. A, vol. 46A, (2015), no. 8, pp. 3581-3591.
116 2015 Diffusion coefficient of gaseous zirconium tetrachloride (ZrCl4) J.H. Shin and J.H. Park Fluid Phase Equilibria, (2015), vol. 389, pp. 4-8. (March).
117 2015 Influence of CaF2 on the viscosity and structure of manganese ferroalloys smelting slags J.H. Park, K.Y. Ko and T.S. Kim Metall. Mater. Trans. B, vol. 46B, (2015), no. 2, pp. 741-748.
118 2015 Effect of CaF2 addition on the silicothermic reduction of MnO in ferromanganese slag J.H. Heo, Y. Chung, and J.H. Park Metall. Mater. Trans. B, vol. 46B, (2015), no. 3, pp. 1154-1161.
119 2015 Thermodynamics of Indium Dissolution Behavior in FeO-bearing Metallurgical Slags Y.S. Han and J.H. Park Metall. Mater. Trans. B, vol. 46B, (2015), no. 1, pp. 235-242.
120 2014 Effect of Al deoxidation on the formation behavior of inclusions in Ce-added stainless steel melt S.K. Kwon, Y.M. Kong, and J.H. Park Met. Mater. Int., vol. 20, (2014), no. 5, pp. 959-966.
121 2014 Mn-depleted zone formation in the rapidly cooled high-strength low-alloy steel welds Y. Kang, K. Han, J.H. Park and C. Lee Metall. Mater. Trans. A, vol. 45A, (2014), no. 11, pp. 4753-4757. (October)
122 2014 Effect of Mg-Ti deoxidation on the formation behaviour of equiaxed crystals during rapid solidification of iron alloys (invited paper, ICS2012 special issue) J.S. Park and J.H. Park Steel Res. Int., vol. 85, (2014), no. 8, pp. 1303-1309.
123 2014 Structure-Viscosity Relationship of Low-silica Calcium Aluminosilicate Melts (invited paper, ATPC2013 special issue) T.S. Kim and J.H. Park ISIJ Int., vol. 54, (2014), no. 9, pp. 2031-2038.
124 2014 Isothermal and non-isothermal sublimation kinetics of zirconium tetrachloride (ZrCl4) for producing nuclear grade Zr J.H. Shin, M.S. Choi, D.J. Min, and J.H. Park Mater. Chem. Phys., vol. 143, (2014), no. 3, pp. 1075-1081. (Feb. 2014)
125 2014 Oxide formation mechanism in high manganese steel welds D. Kim, K. Han, B. Lee, J.H. Park and C. Lee Metall. Mater. Trans. A, vol. 45A, (2014), no. 4, pp. 2046-2054.
126 2014 Effect of Slag Composition on the Concentration of Al2O3 in the Inclusions in Si-Mn-killed Steel J.S. Park and J.H. Park Metall. Mater. Trans. B, vol. 45B, (2014), no. 3, pp. 953-960
127 2014 Influence of Ti on non-metallic inclusion phases and intragranular nucleation in high-strength low-alloy steel weld metals Y. Kang, J. Jang, J.H. Park and C. Lee Met. Mater. Int., vol. 20, (2014), no. 1, pp. 119-127.
128 2013 Effect of CaO Addition on Iron Recovery from Copper Smelting Slags by Solid Carbon J.H. Heo, B.S. Kim and J.H. Park Metall. Mater. Trans. B, vol. 44B, (2013), no. 6, pp. 1352-1363.
129 2013 Conversion of calcium phosphide to calcium phosphate in reducing dephosphorization slags by oxygen injection J.H. Shin and J.H. Park ISIJ Int., vol. 53, (2013), no. 12, pp. 2266-2268.
130 2013 Competitive Dissolution Mechanism of Sulphur in Ca-Mn-Silicate Melts: Structural View (invited paper, MOLTEN2012 special issue) J.H. Park Steel Res. Int., vol. 84, (2013), no. 7, pp. 664-669.
131 2013 Structure-Property relationship of CaO-MgO-SiO2 system: Quantitative analysis of Raman spectra (Marcus A Grossmann Awarded paper) J.H. Park Metall. Mater. Trans. B, vol. 44B, (2013), no. 4, pp. 938-947.
132 2013 Effect of CaF2 addition on the viscosity and structure of CaO-SiO2-MnO slags K.Y. Ko and J.H. Park ISIJ Int., vol. 53, (2013), no. 6, pp. 958-965.
133 2013 Morphologies of alumina nano- and microparticles at the Fe/Al2O3 interface and the effects of reaction time and substrate roughness on size distribution Y.S. Lee, S.M. Jung, J.H. Park and D.J. Min ISIJ Int., vol. 53, (2013), no. 3, pp. 547-549.
134 2013 Effect of silicate structure on thermodynamic properties of calcium silicate melts : Quantitative analysis of Raman spectra J.H. Park Met. Mater. Int., vol. 19, (2013), no. 3, pp. 577-584.
135 2013 Effect of atmosphere and slag composition on the evolution of PH3 gas during cooling of reducing dephosphorization slags J.H. Shin and J.H. Park ISIJ Int., vol. 53, (2013), no. 3, pp. 385-390.
136 2012 Sulfide Capacity and Excess Free Energy of CaO-SiO2-MnO Slag derived from Structural Analysis of Raman Spectra J.H. Park ISIJ Int., vol. 52, (2012), no. 12, pp. 2303-2304.
137 2012 Density Measurements of CaO-MnO-SiO2 Slags J. Lee, L.T. Hoai, J. Choe and J.H. Park ISIJ Int., vol. 52, (2012), no. 12, pp. 2145-2148.
138 2012 Thermodynamics of Reducing Refining of Phosphorous from Si-Mn Alloy using CaO-CaF2 Slag J.H. Shin and J.H. Park Metall. Mater. Trans. B, vol. 43B, (2012), no. 6, pp. 1243-1246.
139 2012 Effect of complex inclusion particles on the solidification structure of Fe-Ni-Mn-Mo alloy J.S. Park, C. Lee, and J.H. Park Metall. Mater. Trans. B, vol. 43B, (2012), no. 6, pp. 1550-1564.
140 2012 Structure–Property Correlations of CaO-SiO2-MnO Slag derived from Raman Spectroscopy J.H. Park ISIJ Int., vol. 52, (2012), no. 9, pp. 1627-1636.
141 2012 Effect of Slag Composition on the Distribution Behavior of Pb between FetO-SiO2(-CaO, Al2O3) Slag and Molten Copper J.H. Heo, S.S. Park and J.H. Park Metall. Mater. Trans. B, vol. 43B, (2012), no. 5, pp. 1098-1105.
142 2012 Composition-structure-property relationships of CaO-MO-SiO2 (M=Mg2+, Mn2+) systems derived from micro-Raman spectroscopy J.H. Park J. Non-Cryst. Solids, vol. 358, (2012), no. 23, pp. 3096-3102. (2012.12)
143 2012 Interfacial reaction between CaO-SiO2-Al2O3-MgO flux and Fe-xMn-yAl (x=10, 20 mass pct, y=1, 3, 6 mass pct) steel melts at 1873 K D.J. Kim and J.H. Park Metall. Mater. Trans. B, vol. 43B, (2012), no. 4, pp. 875-886.
144 2012 Characterization of non metallic inclusions in high manganese and aluminum-alloyed austenitic steels J.H. Park, D.J. Kim, and D.J. Min Metall. Mater. Trans. A, vol. 43A, (2012), no. 7, pp. 2316-2324.
145 2012 Sulfide capacity of the CaO-SiO2-MnO-Al2O3-MgO slags at 1873 K J.H. Park, and G.H. Park ISIJ Int., vol. 52, (2012), no. 5, pp. 764-769.
146 2012 Metastable Phases of Dross Particles Formed in a Molten Zinc Bath and Prediction of Soluble Aluminum during Galvannealing Processes D.J. Paik, M.H. Hong, Y. Huh, J.H. Park, H.G. Chae, S.H. Park, and S.Y. Choun Metall. Mater. Trans. A, vol. 43, (2012), no. 6, pp. 1934-1943.
147 2012 Dissolution Mechanism of Indium in CaO-Al2O3-SiO2 Slag at Low Silica Region K.Y. Ko and J.H. Park Metall. Mater. Trans. B, vol. 43B, (2012), no. 3, pp. 440-442.
148 2012 Influence of aluminum on the formation behavior of Zn-Al-Fe intermetallic particles in zinc bath J.H. Park, G.H. Park, D.J. Paik, Y. Huh and M.H. Hong: Metall. Mater. Trans. A, vol. 43A, (2012), no. 1, pp. 195-207.
149 2011 Dissolution Behavior of Indium in CaO-SiO2-Al2O3 Slag K.Y. Ko and J.H. Park Metall. Mater. Trans. B, vol. 42B, (2011), no. 6, pp. 1224-1230.
150 2011 Effect of inclusions on the solidification structures of ferritic stainless steel: Computational and experimental study of inclusion evolution J.H. Park CALPHAD, vol. 35, (2011), no. 4, pp. 455-462.
151 2011 Solubility of Nitrogen in High Manganese Steel (HMnS) Melts: Interaction Parameter between Mn and N J.H. Shin, J. Lee, D.J. Min, and J.H. Park Metall. Mater. Trans. B, vol. 42B, (2011), no. 6, pp. 1081-1085.
152 2011 On the dissolution behavior of sulfur in ternary silicate slags Y.B. Kang and J.H. Park Metall. Mater. Trans. B, vol. 42B, (2011), no. 6, pp. 1211-1217.
153 2011 Sulfide capacity of the CaO-SiO2-MnO slag at 1873 K G.H. Park, Y.B. Kang and J.H. Park ISIJ Int., vol. 51, (2011), no. 9, pp. 1375-1382.
154 2011 Formation mechanism of MgO×Al2O3 spinel inclusions in stainless steelmaking processes J.H. Park and H. Todoroki J. Iron Steel Res. Int., vol. 18, (2011), suppl. 2, pp. 320-330.
155 2011 Thermodynamics of inclusion formation and its influence on the corrosion behavior of Cu bearing duplex stainless steels S.H. Jeon, S.T. Kim, I.S. Lee, J.H. Park, K.T. Kim, J.S. Kim and Y.S. Park Mater. Trans., vol. 52, (2011), no. 3, pp. 416-422.
156 2011 Effects of copper addition on the formation of inclusions and the resistance to pitting corrosion of high performance duplex stainless steels S.H. Jeon, S.T. Kim, I.S. Lee, J.H. Park, K.T. Kim and Y.S. Park Corros. Sci., vol. 53, (2011), no. 4, pp. 1408-1416.
157 2010 Effect of boron oxide on the crystallization behavior of MgAl2O4 spinel phase during cooling of the CaO-SiO2-10wt%MgO-30wt%Al2O3 systems J.H. Park Met. Mater. Int., vol. 16, (2010), no. 6, pp. 987-992.
158 2010 Studies of the Wetting Characteristics of Liquid Fe-Cr Alloys on Oxide Substrates by the Sessile Drop Technique J. Lee, M. Shin, J.H. Park, and S. Seetharaman Ironmaking & Steelmaking, vol. 37, (2010), no. 7, pp. 512-515. (2010.10)
159 2010 In Situ Observation of Dissolution Phenomena of SiC Particle in the CaO-SiO2-MnO Slag J.H. Park, J.G. Park, D.J. Min, Y.E. Lee and Y.B. Kang J. Eur. Ceram. Soc., vol. 30, (2010), no. 15, pp. 3181-3186. (2010.11)
160 2010 Control of MgO×Al2O3 Spinel Inclusions in Stainless Steels – A review (review paper) J.H. Park and H. Todoroki ISIJ Int., vol. 50, (2010), no. 10, pp. 1333-1346.
161 2010 Interfacial reaction between refractory materials and metallurgical slags containing fluoride (invited paper, Seetharaman Symposium special issue) J.H. Park, M.O. Suk, I.H. Jung, M. Guo and B. Blanpain Steel Res. Int., vol. 81, (2010), no. 10, pp. 860-868.
162 2010 Phosphate Capacity of CaO-SiO2-MnO-FeO Slag saturated with MgO M.K. Cho, J.H. Park and D.J. Min ISIJ Int., vol. 50, (2010), no. 2, pp. 324-326.
163 2010 In-situ Observation of Dynamic Interfacial Phenomena between CaO-(SiO2 or Al2O3) slag and Fe-11%Cr alloy near the MgO-6%C Refractory at 1823K M. Shin, S. Cho, J. Lee and J.H. Park Met. Mater. Int., vol. 16, (2010), no. 3, pp. 495-499.
164 2010 Carbide Capacity of CaO-SiO2-MnO Slag for the Production of Manganese Alloys J.H. Park, G.H. Park and Y.E. Lee ISIJ Int., vol. 50, (2010), no. 8, pp. 1078-1083.
165 2010 A Study on the effect of Na2O on the viscosity of ironmaking slags H. Kim, W.H. Kim, J.H. Park, and D.J. Min Steel Res. Int., vol. 81, (2010), no. 1, pp. 17-24.
166 2010 Hot Metal Desulfurization of CaO-SiO2-CaF2-Na2O Slag saturated with MgO M.K. Cho, J. Cheng, J.H. Park and D.J. Min ISIJ Int., vol. 50, (2010), no. 2, pp. 215-221.
167 2009 Phase Diagram Study for the CaO-SiO2-Cr2O3-5mass%MgO-10mass%MnO System J.H. Park, I.H. Jung and S.B. Lee Met. Mater. Int., vol. 15, (2009), no. 4, pp. 677-681.
168 2009 Electrochemical Method for Controlling the Interfacial Oxygen in Molten Fe with ZrO2 based solid electrolyte W. Kim, D.J. Min, Y.S. Lee and J.H. Park ISIJ Int., vol. 49, (2009), no. 12, pp. 1882-1888.
169 2009 Corrosion Behavior of Zirconia Refractory by CaO-SiO2-MgO-CaF2 Slag M.O. Suk and J.H. Park J. Am. Ceram. Soc., vol. 92, (2009), no. 3, pp. 717-723.
170 2009 Kinetic Study on Surface Dissolution of Nitrogen on Liquid Steel by Isotope Exchange Technique S.M. Han, J.H. Park, S.M. Jung, Jung H. Park, and D.J. Min ISIJ Int., vol. 49, (2009), no. 4, pp. 487-494.
171 2009 Estimation of Sulfur Segregation at the Interface between Molten Iron and Graphite Substrate from Wetting Experiments J. Lee, A. Tazuke, T. Tanaka and J.H. Park Met. Mater. Int., vol. 15, (2009), no. 3, pp. 501-505.
172 2009 Thermodynamics of Titanium Oxide in CaO-SiO2-Al2O3-MgOsatd-CaF2 Slag equilibrated with Fe-11mass%Cr Melt J.H. Park, S.B. Lee, D.S. Kim, and J.J. Pak ISIJ Int., vol. 49, (2009), no. 3, pp. 337-342.
173 2009 Diffusion Kinetics of Oxygen in b-Titanium Measured by Molten Flux Method M.H. Song, S.M. Han, G.S. Choi, D.J. Min, and J.H. Park Metall. Mater. Trans. A, vol. 40, (2009), no. 3, pp. 495-498.
174 2009 Thermodynamics of Copper Dissolution into the MnO-SiO2-MnS Inclusion System J.G. Park, J.H. Park, Y.S. Lee, S.M. Jung, and D.J. Min ISIJ Int., vol. 49, (2009), no. 2, pp. 171-177.
175 2009 Deoxidation thermodynamics of b-titanium by Ca-CaCl2 and Ca-CaF2 fluxes S.M. Han, Y.S. Lee, J.H. Park, G.S. Choi, and D.J. Min Mater. Trans., vol. 50, (2009), no. 1, pp. 215-218.
176 2008 Wetting Characteristics of Liquid Fe-19%Cr-10%Ni Alloys on Dense Alumina Substrates M.S. Shin, J. Lee and J.H. Park ISIJ Int., vol. 48, (2008), no. 12, pp. 1665-1669.
177 2008 A kinetic study of controlling nitrogen in process for boron steel by using 30N2 isotope gas S.M. Han, D.J. Min, J.H. Park, Jung H. Park, and J.M. Park Rev. Metall., (2008), no. 12, pp. 601-608.
178 2008 Diffusion of oxygen in b-titanium M.H. Song, S.M. Han, D.J. Min, G.S. Choi, and J.H. Park Scripta Mater., vol. 59, (2008), no. 6, pp. 623-626.
179 2008 Thermodynamics of the Formation of MgO-Al2O3-TiOx Inclusions in Ti-stabilized 11Cr Ferritic Stainless Steel J.H. Park, S.B. Lee and H.R. Gaye Metall. Mater. Trans. B, vol. 39, (2008), no. 6, pp. 853-861.
180 2008 Thermodynamic investigation on the formation of inclusions containing MgAl2O4 spinel during 16Cr-14Ni austenitic stainless steel manufacturing processes J.H. Park Mater. Sci. Eng. A, vol. 472, (2008), no. 1-2, pp. 43-51.
181 2008 Novel Approach to Link between Viscosity and Structure of Silicate Melts via Darken's Excess Stability Function: Focus on the Amphoteric Behavior of Alumina J.H. Park, H. Kim, and D.J. Min Metall. Mater. Trans. B, vol. 39B, (2008), no. 1, pp. 150-153.
182 2007 Solidification structure of CaO-SiO2-MgO-Al2O3(-CaF2) systems and computational phase equilibria: Crystallization of MgAl2O4 spinel (top 25 hottest articles in CALPHAD 2012 full year) J.H. Park CALPHAD, vol. 31, (2007), no. 4, pp. 428-437.
183 2007 Formation Mechanism of Spinel-type Inclusions in High Alloyed Stainless Steel Melts J.H. Park Metall. Mater. Trans. B, vol. 38B, (2007), no. 4, pp. 657-663.
184 2007 Discussion on "The Estimation of the Iso-viscosity Lines in Molten CaF2-CaO-SiO2 System" J.H. Park and D.J. Min ISIJ Int., vol. 47, (2007), no. 9, pp. 1368-1369.
185 2007 Inclusion Control of Fe-16%Cr Stainless Steel Melts by Aluminum Deoxidation and Calcium Treatment (invited paper, ICS2005 special issue) J.H. Park, D.S. Kim, S.B. Lee, and Y.Y. Lee AIST Trans. in Iron & Steel Technology, vol. 4, (2007), no. 1, pp. 137-144.
186 2007 Thermodynamics of Titanium and Oxygen Dissolved in Liquid Iron Equilibrated with Titanium Oxides J.J. Pak, J.O. Jo, S.I. Kim, W.Y. Kim, T.I. Chung, S.M. Seo, J.H. Park, and D.S. Kim ISIJ Int., vol. 47, (2007), no. 1, pp. 16-24.
187 2007 Formation of CaZrO3 at the Interface between CaO-SiO2-MgO-CaF2(-ZrO2) slags and magnesia refractories: Computational and experimental study (top 25 hottest articles in CALPHAD 2007) J.H. Park CALPHAD, vol. 31, (2007), no. 2, pp. 149-154.
188 2006 Solidification Behavior of Calcium Aluminosilicate Melts containing Magnesia and Fluorspar J.H. Park J. Am. Ceram. Soc., vol. 89, (2006), no. 2, pp. 608-615.
189 2006 Effect of ZrO2 Addition to the CaO-SiO2-MgO-CaF2 Slags on the Sulfur Removal from the 16Cr-14Ni Stainless Steel Melts J.H. Park and D.J. Min Mater. Trans., vol. 47, (2006), no. 8, pp. 2038-2043.
190 2006 Effect of Ferrosilicon Addition on the Composition of Inclusions in 16Cr-14Ni-Si Stainless Steel Melts J.H. Park and Y.B. Kang Metall. Mater. Trans. B, vol. 37B, (2006), no. 5, pp. 791-798.
191 2005 Inclusion Control of Ferritic Stainless Steel by Aluminum Deoxidation and Calcium Treatment J.H. Park, D.S. Kim, and S.B. Lee Metall. Mater. Trans. B, vol. 36B, (2005), no. 1, pp. 67-73.
192 2005 Effect of CaO-Al2O3-MgO Slags on the Formation of MgO-Al2O3 Inclusions in Ferritic Stainless Steel J.H. Park and D.S. Kim Metall. Mater. Trans. B, vol. 36B, (2005), no. 4, pp. 495-502.
193 2004 Effect of fluorspar and alumina on the viscous flow of calcium silicate melts containing MgO J.H. Park and D.J. Min J. Non-Cryst. Solids, vol. 337, (2004), no. 2, pp. 150-156.
194 2004 Thermodynamics of Fluoride Vaporization from Slags containing CaF2 at 1773 K J.H. Park and D.J. Min Steel Res. Int., vol. 75, (2004), no. 12, pp. 807-811.
195 2004 Improvement of Cleanliness of 16%Cr-containing Ferritic Stainless Steel in AOD Processes D.S. Kim, J.H. Park, Jong H. Park, S.B. Lee, and H.G. Lee Rev. Metall., (2004), no. 4, pp. 291-299.
196 2004 Reduction Behavior of EAF Slags containing Cr2O3 using Aluminum at 1793 K J.H. Park, H.S. Song, and D.J. Min ISIJ Int., vol. 44, (2004), no. 5, pp. 790-794.
197 2004 Carbide Capacity of CaO-SiO2-CaF2(-Na2O) Slags at 1773 K J.H. Park and D.J. Min ISIJ Int., vol. 44, (2004), no. 2, pp. 223-228.
198 2004 Amphoteric Behavior of Alumina in Viscous Flow and Structure of CaO-SiO2(-MgO)-Al2O3 Slags J.H. Park, D.J. Min, and H.S. Song Metall. Mater. Trans. B, vol. 35B, (2004), no. 2, pp. 269-275.
199 2002 The Effect of CaF2 on the Viscosities and Structures of CaO-SiO2(-MgO)-CaF2 Slags J.H. Park, D.J. Min and H.S. Song Metall. Mater. Trans. B, vol. 33B, (2002), no. 5, pp. 723-729.
200 2002 Thermodynamic Behavior of Nickel in CaO-SiO2-FetO Slag S.H. Lee, S.M. Moon, J.H. Park, and D.J. Min Metall. Mater. Trans. B, vol. 33B, (2002), no. 1, pp. 55-59.
201 2002 FT-IR Spectroscopic Study on Structure of CaO-SiO2 and CaO-SiO2-CaF2 Slags J.H. Park, D.J. Min, and H.S. Song ISIJ Int., vol. 42, (2002), no. 4, pp. 344-351.
202 2002 Structural Investigation of CaO-Al2O3 and CaO-Al2O3-CaF2 Slags via Fourier Transform Infrared Spectra J.H. Park, D.J. Min, and H.S. Song ISIJ Int., vol. 42, (2002), no. 1, pp. 38-43.
203 2002 Carbide Capacity of CaO-Al2O3-CaF2 Slag at 1773 K J.H. Park, D.J. Min, and H.S. Song ISIJ Int., vol. 42, (2002), no. 2, pp. 127-131.
204 2001 Foaming Behavior of CaO-SiO2-FeO-MgOsatd-X (X=Al2O3, MnO, P2O5, and CaF2) Slags at High Temperatures H.S. Kim, D.J. Min, and J.H. Park Metall. Mater. Trans. B, vol. 32B, (2001), no. 2, pp. 297-303.
205 2001 Sulfide Capacity and Phase Equilibria of MnO-TiO2-MnS System at 1723 K T.G. Kim, W.K. Lee, J.H. Park, D.J. Min, and H.S. Song ISIJ Int., vol. 41, (2001), no. 12, pp. 1460-1464.
206 2001 Thermodynamic Behavior of Na2O-B2O3 Melt J.H. Park and D.J. Min Metall. Mater. Trans. B, vol. 32B, (2001), no. 2, pp. 297-303.
207 2000 Thermodynamic Behavior of Carbon in Molten Slags J.H. Park and D.J. Min ISIJ Int., vol. 40, (2000), suppl., pp. S96-S100.
208 2000 Solubility of Silver in MO(M2O)-B2O3 (M=Ca, Ba, and Na) Slags J.H. Park and D.J. Min Mater. Trans., JIM, vol. 41, (2000), no. 3, pp. 425-428.
209 1999 Solubility of Carbon in CaO-B2O3 and BaO-B2O3 Slags J.H. Park and D.J. Min Metall. Mater. Trans. B, vol. 30B, (1999), no. 6, pp. 1045- 1052.
210 1999 Quantitative Analysis of the Relative Basicity of CaO and BaO by Silver Solubility in Slags J.H. Park and D.J. Min Metall. Mater. Trans. B, vol. 30B, (1999), no. 4, pp. 689-694.
211 1999 Thermodynamic study on the effect of CaF2 on the nitrogen and carbon solubility in the CaO-Al2O3-CaF2 slag system I. Sohn, D.J. Min, and J.H. Park Steel Res., vol. 70, (1999), no. 6, pp. 215-220.